Aqueous magnesium batteries offer low-cost materials, safety, and environmental compatibility, but their anodes suffer from self-corrosion and discharge-product accumulation. These deposits increase internal resistance and lower discharge voltage, making a clean anode surface essential for battery performance. However, achieving both high discharge voltage and anode utilization efficiency requires controlling self-corrosion on the exposed magnesium surface. While the hydrogen evolution reaction (HER) is a recognized cause of self-corrosion, the oxygen reduction reaction (ORR) has received less attention because discharge-product films were thought to restrict oxygen diffusion. Removing these films allows dissolved oxygen to reach the magnesium surface, highlighting the need to investigate ORR and develop targeted electrolyte additive strategies.
Researchers at Helmholtz-Zentrum Hereon, with collaborators at Kiel University and Southeast University, reported (DOI: 10.1016/j.esci.2026.100566) the findings in eScience. The article was available online on Nov. 2026. The team used a magnesium–calcium (Mg–0.2Ca) anode, controlled oxygen levels by gas purging or chemical scavenging, and compared individual additives with binary mixtures. They combined Vit. C with Mg²⁺ complexing agents, including 4-amino-3-hydroxy-1-naphthalenesulfonic acid (4A3HNSA), Tiron, and 3,4-dihydroxybenzoic acid (3,4-DHB). The study linked electrochemical performance to real-time H₂ evolution and interfacial chemistry during discharge.
The study found that ORR can account for a measurable minority—up to roughly one-tenth—of total anodic self-corrosion when Mg²⁺ complexing additives keep the Mg–0.2Ca surface largely film-free. In 4A3HNSA-containing electrolyte, removing dissolved oxygen improved both discharge potential (DP) and utilization efficiency (UE), confirming that dissolved O₂ matters when the surface is clean. The binary mixture of Vit. C and 4A3HNSA delivered better DP and UE than either additive alone and supported stable full-cell discharge over an extended period. Operando microprobes showed lower local dissolved H₂ and pH near the anode in the mixture. X-ray photoelectron spectroscopy (XPS) and vibrational spectroscopy indicated a Mg–N-containing interfacial layer, which the authors link to suppressed HER and mitigated negative difference effect (NDE). The effect was not simply additive: Vit. C removed dissolved O₂, while the complexing agent limited hydroxide deposition and helped preserve a favorable interface. The mixture with Tiron performed poorly, suggesting that excessively strong Mg²⁺ binding can trigger chunk effect. Diffusion-limited ORR currents were low, consistent with ORR’s limited but non-negligible share. Vit. C alone left a visible discharge film and showed little oxygen sensitivity, whereas 4A3HNSA kept the surface clean.
The authors said the key insight is that ORR had been hidden by the assumption that discharge films block oxygen. They said keeping the anode film-free turns dissolved O₂ into a real capacity drain, so the additive design had to solve two problems at once: remove oxygen and manage Mg²⁺ at the interface. They said the binary mixture is more than a simple sum of additives because Vit. C alters the interfacial chemistry and helps form a Mg–N-containing layer that suppresses HER. They added that this coupled mechanism helps explain the simultaneous gains in UE and DP.
The findings offer a practical route for primary aqueous magnesium and magnesium–air (Mg–air) batteries: instead of continuous gas purging, an oxygen-scavenging additive can suppress ORR while a complexing agent keeps the anode clean. The approach may also guide electrolyte design for other metals that face oxygen-driven parasitic reactions. The authors caution that additive strength matters; overly strong Mg²⁺ complexation can increase chunk effect and reduce specific energy. Future work can screen greener oxygen scavengers and pH-buffering agents, optimize additive ratios for different alloys and current densities, and validate long-term performance in full cells. Such formulations could simplify system design where gas purging is impractical. The open-access study provides a mechanistic template for combining additives by function rather than trial and error.
###
References
DOI
10.1016/j.esci.2026.100566
Original Source URL
https://doi.org/10.1016/j.esci.2026.100566
Funding information
Chinese Scholarship Council (CSC) (No. 202106050030 and No. 202206050042); Humboldt Research Fellowship;
About eScience
eScience – a Golden Open Access journal cooperated with KeAi and published online at ScienceDirect. eScience is founded by Nankai University (China) in 2021 and aims to publish high quality academic papers on the latest and finest scientific and technological research in interdisciplinary fields related to energy, electrochemistry, electronics, and environment. eScience provides insights, innovation and imagination for these fields by built consecutive discovery and invention. Now eScience has been indexed by SCIE, EI, CAS, Scopus and DOAJ. Its impact factor is 52.9, which is ranked first in the field of electrochemistry.