□ The world’s first technology for controlling the thickness of a next-generation semiconductor material one atomic layer at a time across an entire 15 cm (6-inch) wafer has been developed. The material is approximately one hundred-thousandth the thickness of a human hair. The research team precisely reduced the material from five layers to four, three, and two layers, and used the thickness-controlled material to develop an artificial intelligence (AI) semiconductor device capable of sensing and remembering light.
□ A research team led by Dr. Hyeong-U Kim, Senior Researcher at the Semiconductor Manufacturing Research Center of the Research Institute of Autonomous Manufacturing at the
Korea Institute of Machinery and Materials (KIMM, President Seog-Hyeon Ryu), in collaboration with Professor Hocheon Yoo’s research team at Hanyang University, developed a technology for controlling 6-inch wafer-scale tungsten disulfide (WS₂) one atomic layer at a time and an AI semiconductor device using the technology. Dr. Kim also serves as an Assistant Professor at the University of Science and Technology (UST) and an Adjunct Professor at Sungkyunkwan University.
□ Tungsten disulfide is a next-generation two-dimensional (2D) semiconductor material consisting of thin atomic layers stacked on top of one another. Because its electrical and optical properties vary depending on the number of layers, it is important to form the desired number of layers uniformly over a large area. However, existing technologies have been limited to small samples or slow processing speeds, making it difficult to uniformly control the thickness of large-area wafers at the atomic-layer level.
□ The research team addressed this limitation using a plasma etching process used in semiconductor manufacturing. The team applied plasma generated from a mixture of three gases to five-layer tungsten disulfide for one to four seconds, selectively removing one atomic layer at a time. Through this process, the team reduced the material from five layers to four, three, and two layers and achieved uniform atomic-layer control down to a semiconductor film thickness of 0.76 nm.
□ This achievement is the result of further advancing the research team’s 2D semiconductor plasma processing technology. The team had previously succeeded in atomic-layer etching of 4-inch molybdenum disulfide (MoS₂). In this study, the team extended the technology to tungsten disulfide and precisely controlled the number of layers from five to two across an entire 6-inch wafer, while also applying the material to an actual AI semiconductor device.
□ The research team also identified the conditions required for uniform etching across a large-area wafer. When the tungsten precursor film used to synthesize the tungsten disulfide had a smoother surface, the atomic layers were removed uniformly one layer at a time. In contrast, when the surface was rougher, some layers were locally damaged and the thickness became non-uniform. Using electron microscopy and other analytical methods, the team confirmed that the surface condition of the initial tungsten film determines the precision of atomic-layer control.
□ Using the tungsten disulfide with its thickness controlled at the atomic-layer level, the research team fabricated an opto-memristor that senses light and remembers previously received light signals. Similar to how the human brain remembers information seen by the eyes, the device combines light sensing and memory functions in a single device. In particular, the four-layer tungsten disulfide device distinguished all 16 possible combinations of four on/off light pulses (4-bit inputs) and stored them as distinct states.
□ The research team also applied the device to reservoir computing, an AI method for processing signals that change over time. In a reservoir computing model based on the measured device characteristics, the system achieved an average accuracy of 95.8% in classifying five types of signal waveforms. The team also confirmed that memory characteristics differed depending on the number of layers. The three-layer device better retained recent input information, while the four-layer device better retained relatively older information. The technology is expected to be used to develop AI semiconductor devices with characteristics suited to different applications by controlling the number of atomic layers.
□ Dr. Hyeong-U Kim, Senior Researcher at KIMM’s Semiconductor Manufacturing Research Center, said, “We confirmed that next-generation semiconductor materials can be controlled one atomic layer at a time across an entire 6-inch wafer, and that the characteristics of AI semiconductor devices can be designed simply by adjusting the material thickness.” He added, “Going forward, we will further develop the technology into low-power AI sensors capable of sensing light and making immediate decisions.”
□ The research was conducted as part of MANUX, KIMM’s flagship research brand for autonomous manufacturing, with support from the KIMM Basic Research Program, the KIMM Strategic Research Program, and K-CHIPS (Korea Collaborative & High-tech Initiative for Prospective Semiconductor Research), funded by the Ministry of Trade, Industry and Energy (MOTIE). The research findings were published in Advanced Functional Materials (IF 19.9, JCR top 4.2%), an international journal in the field of materials science, and were selected for the Back Cover of Vol. 37, Issue 104 in recognition of the originality and impact of the research.
###
The
Korea Institute of Machinery and Materials (KIMM) is a non-profit government-funded research institute under the Ministry of Science and ICT. Since its foundation in 1976, KIMM is contributing to economic growth of the nation by performing R&D on key technologies in machinery and materials, conducting reliability test evaluation, and commercializing the developed products and technologies.